Type: | Stainless Steel Pipes |
---|---|
Standard: | ASTM, AISI, GB |
Grade: | 300 Series |
Certification: | ISO, ASTM, GB, EN |
Shape: | Round |
Technique: | Cold Rolled |
Customization: |
---|
Suppliers with verified business licenses
Grade 304 / 304L stainless steel has a minimum of 18% chromium and 8% nickel. The only difference between them is the carbon content. Type 304 has a maximum carbon of 0.07% .Type 304L has maximum carbon of 0.030 %. This range of carbon in the steels affects the corrosion resistance. 304 / 304L is available in sheet, sheet coil, plate, plate coil, round bar, processed flat bar and tubular products for further manufacturing.
Grade 304 / 304L Stainless Steel is used in a wide variety of commercial and industrial applications, including:
C | Mn | Si | P | S | Cr | Ni | |
304 | 0.07max | 2.0max | 1.00max | 0.045max | 0.03max | min: 17.5 max: 19.5 | min: 8.0 max: 10.5 |
304L | 0.03max | 2.0max | 1.00max | 0.045max | 0.03max | min: 17.5 max: 19.5 | min: 8.0 max: 10.5 |
The properties quoted below are guideline figures only and should not be used for any design purposes.
Grade | Tensile Strength ksi (min) | Yield Strength 0.2% ksi (min) | Elongation % | Hardness (Brinell) MAX |
Hardness (Rockwell B) MAX |
304 / 304L | 75 | 30 | 40 | 201 | 92 |
Density lbm/in3 | Thermal Conductivity (BTU/h ft. °F) | Electrical Resistivity (in x 10-6) | Modulus of Elasticity (psi x 10-6) | Coefficient of Thermal Expansion (in/in)/ °F x 10-6 | Specific Heat (BTU/lb/°F) | Melting Range (°F)) |
at 68°F: 0.285 | 9.4 at 212°F | 28.3 at 68°F | 28 | 9.4 at 32 - 212° | 0.1200 at 68°F to 212°F | 2500 to 2590 |
12.4 at 932 °F | 39.4 at 752°F |
10.2 at 32 - 1000°F |
||||
49.6 at 1652 °F |
10.4 at 32 - 1500°F |
Suppliers with verified business licenses